以热喷涂NiCrBSi涂层/钢基体为材料模型,利用将涂层置于受压侧的反向三点弯曲法试验,对热喷涂涂层界面断裂现象进行分析并建立相应的界面断裂韧性计算模型.结果表明,界面裂纹起始于三点弯曲试样中部,对应于加载压头与涂层接触区域正下方的界面上,并向两侧扩展,伴随涂层屈曲,形成分层屈曲的破坏形貌.根据分层屈曲形貌建立计算模型,通过分层屈曲几何参数与屈曲临界应力、涂层内真实应力以及界面断裂韧性的关系,获得界面断裂韧性值. |
其他语种文摘
|
Interfacial fracture phenomenon was analyzed with three-point reverse bending test to measure the interfacial fracture toughness of thermal spraying NiCrBSi coating/steel substrate.The results show that the interfacial crack initiates along the interface under the contact zone of the indenter and the coating at the mid-span,and buckling morphology is formed as the interfacial crack propagates to two ends of the sample.Calculation model is given according the buckling morphology of the coating,and the interfacial toughness is obtained by the relationship between the geometric parameters of coating buckling and critical stress,real stress and interfacial toughness. |
来源
|
金属热处理
,2010,35(1):114-116 【核心库】
|
关键词
|
三点弯曲试验
;
热喷涂涂层
;
分层屈曲
;
界面断裂韧性
|
地址
|
中国科学院力学研究所, 先进制造工艺力学重点实验室, 北京, 100190
|
语种
|
中文 |
文献类型
|
研究性论文 |
ISSN
|
0254-6051 |
学科
|
金属学与金属工艺 |
基金
|
国家自然科学基金面上项目
|
文献收藏号
|
CSCD:3804794
|
参考文献 共
15
共1页
|
1.
蔡昊. 界面断裂韧性的实验研究.
上海力学,1997,18(3):241-247
|
CSCD被引
3
次
|
|
|
|
2.
杜向鹏. 不锈钢-铝复层材料界面断裂性能分析.
稀有金属材料与工程,2007,36(3):131-133
|
CSCD被引
1
次
|
|
|
|
3.
Ines Hofinger. Effect of substrate surface roughness on the adherence of nicraly thermal spray coatings.
Journal of Thermal Spray Technology,2002,11(3):387-392
|
CSCD被引
1
次
|
|
|
|
4.
郭香华. 叠层结构陶瓷强韧化设计的力学分析.
固体力学学报,2000,21(4):313-324
|
CSCD被引
3
次
|
|
|
|
5.
Huang Zhenyu. Initiation and arrest of an interfacial crack in a four-point bend test.
Engineering Fracture Mechanics,2005,72(17):2584-2601
|
CSCD被引
1
次
|
|
|
|
6.
Limam M. Coating fracture toughness determined by Vickers indentation:an important parameter in cavitation erosion resistance of WCCo thermally sprayed coating.
Surface and Coatings Technology,2004,177:489-496
|
CSCD被引
1
次
|
|
|
|
7.
Kim J J. A new indentation cracking method for evaluating interfacial adhesion energy of hard films.
THIN SOLID FILMS,2003,441(1/2):172-179
|
CSCD被引
2
次
|
|
|
|
8.
Warrender J M. Analysis of thermo-mechanical cracking in refractory coatings using variable pulse-duration laser pulse heating.
WEAR,2007,263:1540-1544
|
CSCD被引
5
次
|
|
|
|
9.
张国祥. 测量镀铬层界面韧性的激光屈曲法.
吉林大学学报:工学版,2008,38(1):57-60
|
CSCD被引
1
次
|
|
|
|
10.
Kachanov L M.
Delamination Buckling of Composite Materials,1988
|
CSCD被引
1
次
|
|
|
|
11.
Hutchinsona J W. The influence of imperfections on the nucleation and propagation of buckling driven delaminations.
Journal of the Mechanics and Physics of Solids,2000,48(4):709-734
|
CSCD被引
1
次
|
|
|
|
12.
Henrik Myher Jensen. Straight-sided,buckling-driven delamination of thin films at high stress levels.
International Journal of Fracture,2001,110(4):371-385
|
CSCD被引
1
次
|
|
|
|
13.
Moon M W. The characterization of telephone cord buckling of compressed thin films on substrates.
Journal of the Mechanics and Physics of Solids,2002,50(11):2355-2377
|
CSCD被引
10
次
|
|
|
|
14.
Je H. Measurement of the noibium/sapphire interface toughness via delamination.
International Journal of Fracture,2003,119(1/2):441-448
|
CSCD被引
1
次
|
|
|
|
15.
Ren F Z. Adhesion strength of Ni film on Ti substrate characterized by three-point bend test,peel test and theoretic calculation.
Materials Science and Engineering A,2006,419(1/2):233-237
|
CSCD被引
3
次
|
|
|
|
|