Inclusions for Ultra-pure Ferritic Stainless Steels Containing 21% Chromium
查看参考文献23篇
文摘
|
As stabilizing elements added into ultra-pure ferritic stainless steels, niobium and titanium react with carbon and nitrogen to form carbonitrides and have great effects on the ratio of equiaxed zone and the grain size of solidification structure of ingots, which remarkably affect the quality of cold-rolled sheets. Combined with thermodynamic calculation, style and precipitation progress of inclusions in ultra-pure ferritic stainless steels were investigated by optical microscopy, scanning electron microscopy, transmission electron microscopy and energy dispersive spectroscopy. The results indicate that the inclusions are mainly Ti-Al-N-O system inclusions in ultra-pure ferritic stainless steels. Al_2O_3 starts to precipitate firstly and then TiO_x and TiN precipitates sequently. The inclusions are mainly single TiN particles and complex inclusions with Al_2O_3-Ti_2O_3 as cores and covered with TiN under the condition of 031% titanium addition and mainly Al2O3 under the condition of 001% titanium addition. A few (Nb,Ti)N particles precipitate because of no enough titanium to react with nitrogen when titanium addition is 001%. In addition, fine Nb(C,N) particles with size of less than 500 nm precipitate at relatively low temperature. |
来源
|
Journal of Iron and Steel Research
, International,2013,20(10):70-74 【核心库】
|
DOI
|
10.1016/s1006-706x(13)60179-x
|
关键词
|
ultra-pure ferritic stainless steel
;
ingot
;
inclusion
;
stabilizing element
|
地址
|
College of Materials and Metallurgy, Northeastern University, Liaoning, Shenyang, 110819
|
语种
|
英文 |
文献类型
|
研究性论文 |
ISSN
|
1006-706X |
学科
|
冶金工业 |
基金
|
Sponsored by Fundamental Research Funds for Central Universities of China
;
国家自然科学基金
|
文献收藏号
|
CSCD:4958492
|
参考文献 共
23
共2页
|
1.
Gardner L. The Use of Stainless Steel in Structures.
Progress in Structural Engineering and Materials,2005,7(2):45
|
CSCD被引
26
次
|
|
|
|
2.
Kim J K. Intergranular Corrosion of Ti-Stabilized 11wt% Cr Ferritic Stainless Steel for Automotive Exhaust Systems.
Corrosion Science,2009,51(11):2716
|
CSCD被引
16
次
|
|
|
|
3.
Fujita N. Effect of Nb on High-Temperature Properties for Ferritic Stainless Steel.
Scripta Materialia,1996,35(6):705
|
CSCD被引
13
次
|
|
|
|
4.
Demiroren H. Corrosion Behavior of Ferritic Stainless Steel Alloyed With Different Amounts of Niobium in Hydrochloric Acid Solution.
Journal of Applied Electrochemistry,2009,39(6):761
|
CSCD被引
2
次
|
|
|
|
5.
Hamada J. Effect of Initial Solidified Structure on Ridging Phenomenon and Texture in Type 430 Ferritic Stainless Steel Sheets.
ISIJ International,2003,43(12):1989
|
CSCD被引
23
次
|
|
|
|
6.
Gordon W. Review of Stabilisation of Ferritic Stainless Steels.
Materials Science and Technology,1996,12(2):126
|
CSCD被引
6
次
|
|
|
|
7.
Basu S. Nozzle Clogging Behaviour of Ti-Bearing Al-Killed Ultra Low Carbon Steel.
ISIJ International,2004,44(10):1653
|
CSCD被引
32
次
|
|
|
|
8.
Shi Caixia. Solidification Structure Refining of 430 Ferrite Stainless Steel With TiN Nucleation.
Journal of Iron and Steel Research, International,2008,15(3):57
|
CSCD被引
9
次
|
|
|
|
9.
Siqueira R P. Composition and Orientation Effects on the Final Recrystallization Texture of Coarse-Grained Nb-Containing AISI 430 Ferritic Stainless Steels.
Materials Science and Engineering, A,2011,528(9):3513
|
CSCD被引
10
次
|
|
|
|
10.
Ozturk B. Thermodynamics of Inclusion Formation in Fe-Cr-Ti-N Alloys.
Metallurgical and Materials Transactions, B,1995,26(3):563
|
CSCD被引
11
次
|
|
|
|
11.
Pak J J. Thermodynamics of TiN Formation in Fe-Cr Melts.
ISIJ International,2005,45(8):1106
|
CSCD被引
18
次
|
|
|
|
12.
Cha W Y. Temperature Dependence of Ti Deoxidation Equilibria of Liquid Iron in Coexistence With Ti_3O_5 and Ti_2O_3.
ISIJ International,2008,48(6):729
|
CSCD被引
4
次
|
|
|
|
13.
Cha W Y. Equilibrium Between Titanium and Oxygen in Liquid Fe-Ti Alloy Coexisted With Titanium Oxides at 1873 K.
ISIJ International,2006,46(7):996
|
CSCD被引
9
次
|
|
|
|
14.
Matsuura H. The Transient Stages of Inclusion Evolution During Al and/or Ti Additions to Molten Iron.
ISIJ International,2007,47(9):1265
|
CSCD被引
14
次
|
|
|
|
15.
Wang C. A Study on the Transient Inclusion Evolution During Reoxidation of a Fe-Al-Ti-O Melt.
ISIJ International,2011,51(3):375
|
CSCD被引
10
次
|
|
|
|
16.
Itoh H. Assessment of AI Deoxidation Equilibrium in Liquid Iron.
Tetsu-to-Hagane, (in Japanese),1997,83(12):773
|
CSCD被引
1
次
|
|
|
|
17.
Liang Yinjiao.
Thermodynamic Data Notebook of Inorganics, (in Chinese),1993
|
CSCD被引
1
次
|
|
|
|
18.
Guo Hanjie.
Tutorial of Metallurgical Physical Chemistry, (in Chinese),2004
|
CSCD被引
1
次
|
|
|
|
19.
Park J H. Thermodynamics of the Formation of MgO-Al_2O_3-TiO_x Inclusions in Ti-Stabilized llCr Ferritic Stainless Steel.
Metallurgical and Materials Transactions, B,2008,39(6):853
|
CSCD被引
12
次
|
|
|
|
20.
Pak J J. Thermodynamics of Titanium and Nitrogen in Fe-Si Melt.
ISIJ International,2005,45(1):23
|
CSCD被引
3
次
|
|
|
|
|