纯Cr和两种含Cr合金在ZnCl2及KCl-ZnCl2盐膜下的腐蚀
Corrosion behavior of pure Cr and two Cr-containing alloys beneath ZnCl_2 and KCl-ZnCl_2 deposits

查看参考文献10篇

文摘 研究了纯Cr、低合金钢及HP型耐热钢在450℃纯氧气氛中分别于在ZnCl2及KCl-ZnCl2盐膜下的腐蚀,结果表明,材料在混合盐膜下比在单一ZnCl2盐膜下发生了更严重的腐蚀,与低合金钢相比,纯Cr和耐热合金中的腐蚀产物更为疏松并易剥落,此外,HP耐热合金中还沿富Cr碳化物发生了晶闸侵蚀,从热力学角度讨论了形成Cr2O3型型保护膜的材料在含氯环境中的脱化机理。
其他语种文摘 The corrosion behavior of pure Cr, one low alloy steel and an HP-type heat-resistant steel were studied in the presence of ZnCl_2 and KCl-ZnCl_2 deposits respectively in oxidizing gaseous environments at 450 ℃. All materials suffered from seriously accelerated corrosion beneath mixture salts than in single ZnCl_2 deposit. The oxide scales formed on pure Cr and heat-resistant steel were easily to spall and had even worse adherence to the matrix compared with that on low alloy steel, whereas the latter had a higher mass gain during corrosion. Furthermore, Cr-rich Cr_7C_3 carbides were attacked preferentially induced by chlorine in comparison to the matrix of the heat resistant steel. The results show that the Cr-containing alloys do not exhibit excellent corrosion resistance to this chlorine-contaminant environment due to the poor adherence of the scales to the matrix. The accelerated corrosion mechanism for those Cr_2O_3-forming materials is discussed thermodynamically.
来源 中国腐蚀与防护学报 ,2002,22(1):27-31 【核心库】
关键词 低合金钢 ; 耐热钢 ; 腐蚀 ; 氯化钾 ; 氯化锌 ;
地址

中国科学院金属研究所, 金属腐蚀与防护国家重点实验室, 辽宁, 110016

语种 中文
文献类型 研究性论文
ISSN 1005-4537
学科 金属学与金属工艺
基金 国家自然科学基金
文献收藏号 CSCD:1136606

参考文献 共 10 共1页

1.  Li Y S. Corrodion Science and Protection Technology,2000,14(2):224-227 被引 1    
2.  Grabke H J. Corros.Sci.,1995,37(7):1023-1043 被引 37    
3.  Li Y S. Acta Metallurgica Sinica (in Chinese) ,2000,36(11):1183-1186 被引 1    
4.  Li Y S. Rare Metal Materials and Enginering.Accepted 被引 1    
5.  Shinata Y. Mater.Sci.Eng.,1987,87:399-405 被引 15    
6.  Zaha A. Mater.Corros.,1999,50:561-578 被引 1    
7.  Rapp R A. Corrosion,1986,42(10):568-577 被引 5    
8.  Ishitsuka R. Mater.Corros,2000,51(3):177-181 被引 1    
9.  Otsuka N. High temperature corrosion of advanced naterials and protective coatings,1992:205-211 被引 1    
10.  Takemura M. Environmental effects on molten chlorides accelerated corrosion in waste incineration systems 被引 1    
引证文献 8

1 马海涛 铁基合金在KCl盐膜下的腐蚀 材料保护,2003,36(1):5-7
被引 1

2 郭贵芬 KCI蒸汽对纯Ni材高温氧化行为的影响 材料保护,2003,36(10):18-20
被引 1

显示所有8篇文献

论文科学数据集
PlumX Metrics
相关文献

 作者相关
 关键词相关
 参考文献相关

版权所有 ©2008 中国科学院文献情报中心 制作维护:中国科学院文献情报中心
地址:北京中关村北四环西路33号 邮政编码:100190 联系电话:(010)82627496 E-mail:cscd@mail.las.ac.cn 京ICP备05002861号-4 | 京公网安备11010802043238号