文摘 随着锂离子电池能量密度进一步提高, 成本进一步降低, 其应用领域越来越广泛, 特别是最近几年来在电动汽车和储能领域的应用被寄予厚望. 然而, 锂离子电池的安全性是目前制约其应用领域扩展的主要瓶颈之一. 锂离子电池的安全性归根结底取决于锂离子电池材料的热稳定性, 本文综述了锂离子电池材料热稳定性的理解和提高方面的最新进展. 过充、热箱、针刺、挤压和内短路是最为关键和具有代表性的安全测试项目, 本文在结合本课题组研究成果的基础上讨论了影响这些安全测试项目的影响因素, 并总结了改善锂离子电池安全性能的方法
其他语种文摘 Application of lithium ion battery (LIB) has been widely extended as its energy density is improved and its cost is reduced. Especially in recent years, significant attention has been paid to application of LIB in electric vehicles and energy storage. However, safety performance of LIB is considered as one of the major barriers which impede the expansion of these application fields. Since safety performance of LIB is fundamentally determined by thermal stability of materials for lithium-ion battery, this paper reviews recent research progress in this field. Among all of the safety tests, overcharge, hot box, nail penetration, crush and internal short are usually considered to be critical ones. This paper discusses major factors influencing these safety tests based on research results obtained in the authors'group. This paper also summarizes state-of-the-art approaches to improve safety performance of LIB in terms of battery materials, cell design and manufacturing
来源 化学进展 ,2011,23(2/3):401-409 【核心库】
关键词 锂离子电池 ; 热稳定性 ; 安全性 ; 过充 ; 热箱 ; 短路
地址

1. 上海交通大学化学化工学院, 上海, 200240  

2. 东莞新能源科技有限公司, 东莞, 523808

语种 中文
文献类型 研究性论文
ISSN 1005-281X
学科 电工技术
基金 国家973计划
文献收藏号 CSCD:4191816

参考文献 共 59 共3页

1.  胡广侠. 影响锂离子电池安全性的因素. 电化学,2002,8(3):245-250 CSCD被引 15    
2.  王静. 锂离子电池安全性研究进展. 电池,2003,33(6):388-391 CSCD被引 14    
3.  Spotnitz R. J. Power Sources,2003,113:81-100 CSCD被引 130    
4.  王青松. 锂离子电池热安全性的研究进展. 电池,2005,35(3):240-241 CSCD被引 12    
5.  唐致远. 化学进展,2006,36(1):74-76 CSCD被引 1    
6.  Balakrishnan P G. J. Power Sources,2006,155:401-414 CSCD被引 79    
7.  Du Pasquier A. J. Electrochem. Soc,1998,145(2):472-477 CSCD被引 11    
8.  Zhang Z. J. Power Sources,1998,70(1):16-20 CSCD被引 35    
9.  Maleki H. J. Electrochem. Soc,1999,146(9):3224-3229 CSCD被引 35    
10.  Richard M N. J. Electrochem. Soc,1999,146(6):2068-2077 CSCD被引 38    
11.  MacNeil D D. J. Electrochem. Soc,1999,146(10):3596-3602 CSCD被引 13    
12.  Andersson A M. Electrochim. Acta,2002,47:1885-1898 CSCD被引 17    
13.  Roth E P. J. Power Sources,2004,134:222-234 CSCD被引 10    
14.  Jiang J W. Electrochim. Acta,2004,49:4599-4604 CSCD被引 8    
15.  Watanabe I. J. Power Sources,2006,153:402-404 CSCD被引 3    
16.  Yang H. J. Power Sources,2007,167:515-519 CSCD被引 13    
17.  Biensan P. J. Power Sources,1999,81/82:906-912 CSCD被引 65    
18.  Dahn J R. Solid State Ionics,1994,69(3/4):265-270 CSCD被引 54    
19.  Veluchamy A. J. Power Sources,2009,189:855-858 CSCD被引 11    
20.  MacNeil D D. J. Electrochem. Soc,2001,148(11):A1211-A1215 CSCD被引 34    
引证文献 22

1 柯佳颖 锂离子电池隔膜材料中离子扩散问题的随机行走模拟 复旦学报. 自然科学版,2012,51(2):251-254,258
CSCD被引 3

2 李毅 锂离子电池火灾危险性研究 中国安全科学学报,2012,22(11):36-41
CSCD被引 15

显示所有22篇文献

论文科学数据集
PlumX Metrics
相关文献

 作者相关
 关键词相关
 参考文献相关

版权所有 ©2008 中国科学院文献情报中心 制作维护:中国科学院文献情报中心
地址:北京中关村北四环西路33号 邮政编码:100190 联系电话:(010)82627496 E-mail:cscd@mail.las.ac.cn 京ICP备05002861号-4 | 京公网安备11010802043238号